A study of the radiation tolerance of cvd diamond to 70 mev protons, fast neutrons and 200 mev pions

التفاصيل البيبلوغرافية
العنوان: A study of the radiation tolerance of cvd diamond to 70 mev protons, fast neutrons and 200 mev pions
المؤلفون: Bäni, L., Alexopoulos, A., Artuso, M., Bachmair, F., Bartosik, M. R., Beck, H. C., Bellini, V., Belyaev, V., Bentele, B., Bes, A., Brom, J.-M., Chiodini, G., Chren, D., Cindro, V., Claus, G., Collot, J., Cumalat, J., Curtoni, S., Dabrowski, A. E., D’alessandro, R., Dauvergne, D., De Boer, W., Dorfer, C., Dünser, M., Eigen, G., Eremin, V., Forneris, J., Gallin-Martel, L., Gallin-Martel, M.-L., Gan, K. K., Gastal, M., Ghimouz, A., Goffe, M., Goldstein, J., Golubev, A., Gorišek, A., Grigoriev, E., Grosse-Knetter, J., Grummer, A., Hiti, B., Hits, D., Hoeferkamp, M., Hosselet, J., Hügging, F., Hutson, C., Janssen, J., Kagan, H., Kanxheri, K., Kass, R., Kis, M., Kramberger, G., Kuleshov, S., Lacoste, A., Lagomarsino, S., Lo Giudice, A., Paz, I. L., Lukosi, E., Maazouzi, C., Mandić, I., Marcatili, S., Marino, A., Mathieu, C., Menichelli, M., Mikuž, M., Morozzi, A., Moscatelli, F., Moss, J., Mountain, R., Oh, A., Olivero, P., Passeri, D., Pernegger, H., Perrino, R., Picollo, F., Pomorski, M., Potenza, R., Quadt, A., Rarbi, F., Re, A., Reichmann, M., Roe, S., Rossetto, O., Becerra, D. A. S., Schmidt, C. J., Schnetzer, S., Sciortino, S., Scorzoni, A., Seidel, S., Servoli, L., Smith, D. S., Sopko, B., Sopko, V., Spagnolo, S., Spanier, S., Stenson, K., Stone, R., Stugu, B., Sutera, C., Traeger, M., Trischuk, W., Truccato, M., Tuvè, C., Velthuis, J., Wagner, S., Wallny, R., Wang, J., Wermes, N., Wickramasinghe, J., Yamouni, M., Zalieckas, J., Zavrtanik, M., Hara, K., Ikegami, Y., Jinnouchi, O., Kohriki, T., Mitsui, S., Nagai, R., Terada, S., Unno, Y., Collaboration, RD42
المصدر: Sensors, 20 (22), Art.-Nr.: 6648 ; ISSN: 1424-8220
بيانات النشر: MDPI
سنة النشر: 2020
المجموعة: KITopen (Karlsruhe Institute of Technologie)
مصطلحات موضوعية: Chemical Vapor Deposition, single-crystalline diamond, polycrystalline diamond, charge collection distance, mean drift path, schubweg, radiation tolerance, radiation damage constant, ddc:530, Physics, info:eu-repo/classification/ddc/530
الوصف: We measured the radiation tolerance of commercially available diamonds grown by the Chemical Vapor Deposition process by measuring the charge created by a 120 GeV hadron beam in a 50 μm pitch strip detector fabricated on each diamond sample before and after irradiation. We irradiated one group of samples with 70 MeV protons, a second group of samples with fast reactor neutrons (defined as energy greater than 0.1 MeV), and a third group of samples with 200 MeV pions, in steps, to (8.8±0.9) × 10$^{15}$ protons/cm$^{2}$, (1.43±0.14) × 10$^{16}$ neutrons/cm$^{2}$, and (6.5±1.4) × 1014 pions/cm$^{2}$, respectively. By observing the charge induced due to the separation of electron–hole pairs created by the passage of the hadron beam through each sample, on an event-by-event basis, as a function of irradiation fluence, we conclude all datasets can be described by a first-order damage equation and independently calculate the damage constant for 70 MeV protons, fast reactor neutrons, and 200 MeV pions. We find the damage constant for diamond irradiated with 70 MeV protons to be 1.62±0.07(stat)±0.16(syst)× 10−18 cm$^{2}$/(pμm), the damage constant for diamond irradiated with fast reactor neutrons to be 2.65±0.13(stat)±0.18(syst)× 10−18 cm$^{2}$/(nμm), and the damage constant for diamond irradiated with 200 MeV pions to be 2.0±0.2(stat)±0.5(syst)× 10−18 cm$^{2}$/(πμm). The damage constants from this measurement were analyzed together with our previously published 24 GeV proton irradiation and 800 MeV proton irradiation damage constant data to derive the first comprehensive set of relative damage constants for Chemical Vapor Deposition diamond. We find 70 MeV protons are 2.60 ± 0.29 times more damaging than 24 GeV protons, fast reactor neutrons are 4.3 ± 0.4 times more damaging than 24 GeV protons, and 200 MeV pions are 3.2 ± 0.8 more damaging than 24 GeV protons. We also observe the measured data can be described by a universal damage curve for all proton, neutron, and pion irradiations we performed of Chemical Vapor ...
نوع الوثيقة: article in journal/newspaper
وصف الملف: application/pdf
اللغة: English
العلاقة: info:eu-repo/semantics/altIdentifier/issn/1424-8220; https://publikationen.bibliothek.kit.edu/1000126944Test; https://publikationen.bibliothek.kit.edu/1000126944/94361140Test; https://doi.org/10.5445/IR/1000126944Test
DOI: 10.5445/IR/1000126944
الإتاحة: https://doi.org/10.5445/IR/1000126944Test
https://doi.org/10.3390/s20226648Test
https://publikationen.bibliothek.kit.edu/1000126944Test
https://publikationen.bibliothek.kit.edu/1000126944/94361140Test
حقوق: https://creativecommons.org/licenses/by/4.0/deed.deTest ; info:eu-repo/semantics/openAccess
رقم الانضمام: edsbas.7E569DAA
قاعدة البيانات: BASE