Preliminary Investigation of the Feasibility of Using a Superpave Gyratory Compactor to Design Cement-Treated Aggregate Mixture

التفاصيل البيبلوغرافية
العنوان: Preliminary Investigation of the Feasibility of Using a Superpave Gyratory Compactor to Design Cement-Treated Aggregate Mixture
المؤلفون: Pusheng Liu, Yinfei Du, Jian Zhang, Yu Zheng, Tian Jun
المصدر: Applied Sciences
Volume 8
Issue 6
Applied Sciences, Vol 8, Iss 6, p 946 (2018)
بيانات النشر: MDPI AG, 2018.
سنة النشر: 2018
مصطلحات موضوعية: Materials science, locking point, 0211 other engineering and technologies, Compaction, Maximum dry density, 02 engineering and technology, lcsh:Technology, Gyration, lcsh:Chemistry, Asphalt pavement, 021105 building & construction, 0502 economics and business, General Materials Science, Geotechnical engineering, lcsh:QH301-705.5, Instrumentation, Fluid Flow and Transfer Processes, Cement, 050210 logistics & transportation, Aggregate (composite), lcsh:T, Process Chemistry and Technology, 05 social sciences, General Engineering, cement-treated aggregate mixture, lcsh:QC1-999, Computer Science Applications, Vibration, Superpave gyratory compactor, Compressive strength, lcsh:Biology (General), lcsh:QD1-999, lcsh:TA1-2040, compaction level, lcsh:Engineering (General). Civil engineering (General), lcsh:Physics
الوصف: Cement-treated aggregate mixture (CTAM) is widely used in many countries. To design this mixture using the vibration compaction method brings about many problems, such as serious inconsistencies in key parameters and strong vibration energy and noise imposed on adjacent buildings and people. This work presents a preliminary investigation of the use of Superpave gyratory compactor, which has been widely used to compact hot mix asphalt in the laboratory, to design CTAM. The 3-2-2 mode of the locking point was used to determine that the gyration compaction number Ndesign should be 105. The performances of the CTAM specimens prepared using gyration compaction were compared with those prepared using the Proctor and vibration compaction methods. Compared with Proctor and vibration compaction, gyration compaction had a smaller influence on aggregate degradation. Also, the optimal moisture content after gyration compaction was the minimum. The index values for maximum dry density, unconfined compressive strength and dry/temperature shrinkage coefficient after gyration compaction were between those for Proctor compaction and vibration compaction. It can be concluded that it is feasible to design CTAM by using a Superpave gyratory compactor to compact the mixture for 105 cycles.
وصف الملف: application/pdf
تدمد: 2076-3417
الوصول الحر: https://explore.openaire.eu/search/publication?articleId=doi_dedup___::82d1a568d6fa1b907f288b6736c520c4Test
https://doi.org/10.3390/app8060946Test
حقوق: OPEN
رقم الانضمام: edsair.doi.dedup.....82d1a568d6fa1b907f288b6736c520c4